Skip to main content
. 2020 Jun 9;6(6):e04177. doi: 10.1016/j.heliyon.2020.e04177

Table 3.

Band gap energy, Urbach energy and electron-phonon interaction of PVC-PS, PVC-PS-SiO2 5% and PVC-PS-SiO2 10% thin films.

Parameter Symbol PVC-PS PVC-PS-5%silica PVC-PS-10%silica
Average Thickness (nm) d 300 300 300
Thickness determined using our model (nm) d 292.597 306.035 302.351
Band gap energy from Tauc plot (eV) Eg,Tauc 3.993 4.002 4.003
Band gap energy from our model (eV) Eg 3.835 3.961 4.133
Urbach energy (meV) EU 356 1067 1066
Steepness parameter (eV−1) σ 0.0726 0.0242 0.0243
Electron-phonon interaction (eV) Eep 9.183 27.548 27.435