Skip to main content
. 2020 May 15;13(10):2284. doi: 10.3390/ma13102284

Figure 2.

Figure 2

Physical appearance of metakaolin/cordierite geopolymers after firing at 800 °C/2 h, with increasing cordierite addition (from 0 to 50 wt.%). Reprinted from [53] under the license n. 4792970655838.