Compositions and properties of pastes derived from the alkali activation of pure and mixed alumino-silicate and carbonate muds [45,46].

Pure Alumino-Silicate Mixed
Alumino-Silicate/Carbonate
Mixed
Carbonate/Silica
Pure Carbonate
Composition 100% granite ~70% granite 95.4% marble 100% marble
~30% dolomite 4.6% waste glass
28 day compressive strength ~30 MPa ~30 MPa ~45 MPa >35 MPa
28 day flexural strength ~12 MPa ~14 MPa ~17 MPa ~11 MPa
Water resistance Rapid dissolution Crack formation Optimal behavior Crack formation