. 2020 May 20;13(10):2348. doi: 10.3390/ma13102348

Figure 4.

Figure 4

Optical micrograph of microstructures after compression with εt of (a) 0, (b) −0.22, (c) −0.40 (d) −0.69, and (e) −1.11 at 350 °C and 10 s−1. Yellow ellipses highlight refined DRXed grains formed near the Zr-rich coarse grains.