Skip to main content
. 2020 May 21;13(10):2368. doi: 10.3390/ma13102368

Figure 5.

Figure 5

(a) Photo of specimen MB_300_60_B_F_3 before the beginning of the test. Load responses of specimen (b) MB_300_60_B_F_1, (c) MB_300_60_B_F_2, and (d) MB_300_60_B_F_3. (e) Failure of PBO fibers and (f) global slip vs. number of cycles for specimen MB_300_60_B_F_3.