Skip to main content
. 2020 May 20;13(10):2359. doi: 10.3390/ma13102359

Figure 13.

Figure 13

Comparison of the coefficient of friction for the material X37CrMoV5-1, ZrO2 ball as a counterpart, and 90 N load. (a) Sample in the basic annealed state. (b) Sample after hardening and being tempered.