Skip to main content
. 2020 May 26;5(22):12682–12691. doi: 10.1021/acsomega.9b04205

Table 1. Thermal Decomposition of the PVDF Nanocomposite-Based Flexible Strain Sensor.

polymer nanocomposites T5% (°C) T30% (°C) THRI (°C)a
PVDF 438.96 466.31 223.1
PVDF/HEG 446.51 470.4 225.8
PVDF/PSS-HEG 456.61 477.6 229.9
a

THRI = 0.49 [T5% + 0.6 (T30%T5%)],45 where T5% and T30% are decomposition temperatures for 5% and 30% weight loss, respectively.