Table 1. Calculated Parameters for Bentonite/E and Bentonite/W at Different Polymer Concentrations Using Bingham Plastic, Power-Law, and Herschel–Bulkley Models.
E-AM/AMPS concentration (wt %) |
W-AM/AMPS concentration (wt %) |
||||||||
---|---|---|---|---|---|---|---|---|---|
models | 0.5 | 1 | 1.5 | 2 | 0.5 | 1 | 1.5 | 2 | |
Bingham model | τ0 | 1.52025 | 2.14563 | 2.82927 | 3.58309 | 1.08489 | 1.52038 | 2.16113 | 1.96954 |
μp | 0.01034 | 0.01788 | 0.02787 | 0.04168 | 0.00713 | 0.01235 | 0.01809 | 0.02476 | |
R2 | 0.9898 | 0.98354 | 0.97741 | 0.97312 | 0.99179 | 0.99299 | 0.9885 | 0.99249 | |
RMSE | 0.4043 | 0.8909 | 1.63 | 2.664 | 0.2498 | 0.3999 | 0.7516 | 0.8302 | |
power-law model | n | 0.63811 | 0.66756 | 0.68404 | 0.69888 | 0.63642 | 0.69036 | 0.68279 | 0.76416 |
K | 0.13798 | 0.1905 | 0.26041 | 0.34635 | 0.09674 | 0.11352 | 0.17404 | 0.13242 | |
R2 | 0.97735 | 0.99124 | 0.99719 | 0.99965 | 0.97174 | 0.98233 | 0.98557 | 0.99533 | |
RMSE | 0.6024 | 0.6499 | 0.5745 | 0.306 | 0.4635 | 0.6347 | 0.8417 | 0.6545 | |
Herschel–Bulkley model | n | 0.81914 | 0.77474 | 0.74015 | 0.71639 | 0.83944 | 0.84792 | 0.81879 | 0.84297 |
K | 0.03655 | 0.08641 | 0.17189 | 0.30416 | 0.02185 | 0.03568 | 0.0641 | 0.07408 | |
τ0 | 1.08587 | 1.15883 | 0.97629 | 0.46345 | 0.82505 | 1.09776 | 1.40014 | 1.0896 | |
R2 | 0.99967 | 0.9996 | 0.9995 | 0.99985 | 0.99936 | 0.99992 | 0.99759 | 0.9999 | |
RMSE | 0.07309 | 0.1391 | 0.2435 | 0.2 | 0.07 | 0.0424 | 0.3443 | 0.09349 |