Table 2.
Sample | Density (g/cm3) | Maximal relative deformation, εdestr | Strength σc (Mpa) | Young’s modulus E (GPa) |
---|---|---|---|---|
HA-alginate | 2.03 ± 0.03 | 0.17 ± 0.01 | 159 ± 7 | 0.563 ± 0.020 |
HA-alginate-0.05SWCNT | 2.02 ± 0.03 | 0.19 ± 0.01 | 166 ± 7 | 0.570 ± 0.020 |
HA-alginate-0.5SWCNT | 2.04 ± 0.04 | 0.28 ± 0.01 | 202 ± 9 | 0.645 ± 0.028 |
*p ≤ 0.05