Skip to main content
. 2020 Jun 17;6(25):eabb1122. doi: 10.1126/sciadv.abb1122

Fig. 6. Electrochemical reversibility of Zn electrodeposits measured in a 2.5 M ZnSO4 (aq) electrolyte.

Fig. 6

(A) Coulombic efficiency for Zn plating/stripping with and without rotation. (B) Coulombic efficiency for Zn plating/stripping at different RDE rotation rates. Time-dependent evolution of the current density during stripping of Zn deposited (C) with and (D) without normal flow.