Skip to main content
. 2020 Jun 12;6(6):e04186. doi: 10.1016/j.heliyon.2020.e04186

Figure 7.

Figure 7

MB degradation spectral profiles of undoped ZnO (a), 2 at.% Mn doped ZnO (b) and 6 at.% Mn doped ZnO (c) photocatalysts. Bottom right (d) is a plot of UV shielding performance (I) in percentage as a function of time for the three photocatalysts.