authors material laser pulses CHF (kW m–2) ΔCHF (%) h (kW m–2 K–1) Δh (%)
Kruse et al.26 stainless steel fs 1420 +56 67.4 +193
Kruse et al.64 copper fs 1300a –22 70.3a +1
Kruse et al.65 copper fs 1430 –15 87.0 +24
Nirgude and Sahu27 copper ns N/Ab N/A 41.5b +80
Zupančič et al.28 stainless steel ns N/Ab N/A 35.4b +177
Voglar et al.29 stainless steel ns 1200c +269 48.2c +166
Može et al.30 copper ns 1580 +89 76.1 +129
Mani et al.66 copper ps 2260 +103 97.5 +153
this study aluminum ns 1539 +41 201.4 +496
a

Only surfaces without microchannels are considered.

b

CHF not measured, HTC at the highest heat flux measured on an individual surface.

c

Thin heater burnout.