Skip to main content
. 2020 Jun 24;11:3185. doi: 10.1038/s41467-020-17044-4

Fig. 1. Morphological study of the Ru/TiO2 catalysts.

Fig. 1

a Elemental mapping of Ru/Ti/O in the fresh Ru/TiO2 catalyst. b HAADF-STEM image of the Ru/TiO2 catalyst pretreated at 600 °C (Ru/TiO2-600 sample) with the metal size distribution. c HRTEM image of the Ru/TiO2-600 catalyst.