Fig. 2. The evolution of Ru/TiO2 catalysts reduced at different temperatures.

Fig. 2

a Fourier transforms of the k3-weighted EXAFS of Ru K-edge for Ru foil, RuO2, and the Ru/TiO2 catalysts pretreated at different temperatures (Ru/TiO2-x samples). b Ti L3,2-edge XANES for the Ru/TiO2 catalysts pretreated at different temperatures (Ru/TiO2-x samples). c A schematic illustration of the structural evolution of Ru/TiO2 at different stages of reduction.