Skip to main content
. 2020 Jun 12;5(24):14535–14542. doi: 10.1021/acsomega.0c01239

Table 3. Switching Speed Comparison with Various Devices Incorporating Hot Carrier Generated by Nanoplasmonic Effects.

  response time (switching speed)
 
devices rise time (ms) decay time (ms) references
Au NPs/GaN-NF/Si(111) 40 40 this work
Au NPs/GaN-NS/Si(111) 40 40 this work
Au NP/Ga-polar GaN 2900 6200 (40)
Au NP/ZnO/PET 10,300 14,200 (41)
Ag-NP/ZnO-NW 80 3270 (42)
Pt-NP/GaN-NS/Al2O3 1100 650 (7)
ZnO-NP/quartz 600 8000 (43)
ZnO-NP/quartz 22,000 11,000 (44)
ZnO-NP/glass 2000 12,000 (45)
TiO2-NP/SiOx 1000 900 (46)
TiO2-nanofibers/SiO2/Si 1500 7800 (47)