Table 5.
SHG intensity of a La3B6O13(OH) powder sample compared with the three reference materials.
Compound |
SHG Intensity [mV] |
I SHG/I Quartz*100 % |
---|---|---|
α‐Al2O3 |
0.2 (0.2) |
0.6 |
Quartz |
31.0 (9.9) |
100 |
KDP (KH2PO4) |
296.9 (31.1) |
958 |
La3B6O13(OH) |
19.7 (17.6) |
63 |