Figure 1.
Schematic illustration of the raw material and all the other samples after the extraction steps. The weight of the raw material (A) after washing and drying it in the oven at 50 °C for 24 h was 5.4 g. The weight of dried demineralized (B), deproteinized (C), and decolorized samples (chitin-D) was 4.6, 3.2, and 2.3 g, respectively.