Dimensional and chemical-physical data of AuNP coated with charged polymers.

AuNP@HS-PEGCOO(−) AuNP@HS-PEGCOO(−)/PAH(+) AuNP@HS-PEGCOO(−)/PAH(+)/PSS(−)
rhyd(nm)a 58(2) 178(8) 197(6)
ζ (mv) −22(2) +36(2) −27(3)
%w/wb 12.27(4)
Au: 86.61(4)
18.17(3)
Au: 76.73(3)
20.27(4)
Au: 74.46(4)
Au concc 1.07 × 10−3 M (0.211 mg/mL) 7.88 × 10− 4M
(0.155 mg/mL)
9.38 × 10−4M
(0.185 mg/mL)
λmax(nm)d 524 534 526

a Hydrodynamic radius determined in water. b % of organic material and % of gold in the dry products, determined by TGA; water is adsorbed on the solid samples, the % Au is calculated by subtracting the % of organic matter and % of water to 100; c Au concentration (by ICP-OES) in the 10-fold preconcentrated aqueous solutions, before ink formation; d maximum of absorption measured in the ink solvent mixture.