Polymer type | Chemical structure | Polymer density (g/cm3) | Commonly used saturated salt solution for density separation | Shaking time | Settling time | Recovery rate | References |
---|---|---|---|---|---|---|---|
PE | 0.92-0.97 | NaCl (1.2 g/cm) | 3 min | 10 min | > 85.0% | Quinn et al. (2016) | |
PP | 0.90-0.91 | ZnCl2 (1.5 g/cm) | 10 min | 15 min | > 95.0% | Rodrigues et al. (2020) | |
PS | 1.04-1.10 | ZnCl2 (1.5 g/cm) | 5 min stirring + 5 min rest + 3 short stirring bursts | overnight | 96.3% | Vermeiren et al. (2020) | |
PVC | 1.16-1.58 | ZnCl2 (1.5 g/cm) | 5 min stirring + 5 min rest + 3 short stirring bursts | overnight | 82.8% | Vermeiren et al. (2020) | |
PET | 1.37-1.45 | ZnBr2 (1.7 g/cm3) | 3 min | 10 min | > 95.0% | Quinn et al. (2016) |