Skip to main content
. 2020 Jun 24;11:1389. doi: 10.3389/fmicb.2020.01389

TABLE 1.

Mass losses comparing unmodified wood or wood that was PAA-delignified and then treated with either 1, 2, or 4 pulses of the CMF system.

Samples CMF Mass loss
Unmodified Wood 1-pulse 4%
2-pulses 16%
4-pulses 78%
Delignified wood 1-pulse 33%
2-pulses 36%

Only single samples were available for the mass loss measurements.