. 2020 Jun 17;5(25):14924–14932. doi: 10.1021/acsomega.0c00198

Table 4. Changes of Light and Heavy Components after Tar Cracked by Different ZnO Loadings.

  ZnO loading
  coal PC HPC ZHPC-5% ZHPC-10% ZHPC-15%
light component (g) 0.3551 0.4390 0.4537 0.3724 0.3659 0.3685
heavy component (g) 0.9689 0.7620 0.5512 0.2504 0.2369 0.2978
light component ratio (%) 26.8 36.55 45.15 59.80 60.70 55.31