Figure 4.

Figure 4.

X-ray diffractograms (Fe Kα radiation, λ = 1.9373 Å) of industrial nano-ZnO (nZnO, black), sunscreen nZnO (red), algae-industrial nZnO (blue), and algae-sunscreen nZnO (green)