Skip to main content
. 2020 Jul 4;5(4):1004–1017. doi: 10.1016/j.bioactmat.2020.06.011

Table 2.

The Ca/P ratio of apatite deposition on various specimens after immersion in SBF for 21 days evaluated by EDX.

SPEEK-5 SPEEK-15 SPEEK-30 SPEEK-60 SPEEK-90
Ca (mol) 0.787 ± 0.065 0.782 ± 0.044 0.684 ± 0.037 0.738 ± 0.032 0.669 ± 0.042
P (mol) 0.480 ± 0.041 0.475 ± 0.025 0.418 ± 0.020 0.450 ± 0.027 0.405 ± 0.032
Ca/P 1.640 ± 0.022 1.640 ± 0.013 1.640 ± 0.009 1.640 ± 0.017 1.650 ± 0.019