Skip to main content
. 2020 Jun 17;13(12):2750. doi: 10.3390/ma13122750

Figure 4.

Figure 4

(A) The rheological parameters (e.g., G′ and G″) for all tested HS-IPN hydrogels increased with increasing the weight ratios of SF/HA in producing the hydrogels versus the varying angular frequencies, (B) increasing weight ratios of SF/HA in the HS-IPN hydrogels increased the δ values from about 4.2 (e.g., HS1-IPN) hydrogels to 8.0° (e.g., HS7-IPN) hydrogels vs. with varying angular frequencies, respectively (Data are mean ± SD, n = 3).