Skip to main content
. 2020 Jun 18;13(12):2763. doi: 10.3390/ma13122763

Figure 15.

Figure 15

Efficiency of UV-Vis phenol degradation in the presence of a defective TBT-HIO3_50 photocatalyst measured in the three subsequent cycles.