Skip to main content
. 2020 Jun 18;13(12):2763. doi: 10.3390/ma13122763

Table 5.

Crystalline phases characteristic for the obtained defective TiO2-HIO3 samples.

Sample Crystalline Size and Phase Content
Anatase Rutile Brookite
Size (nm) Phase Content (wt%) Size (nm) Phase Content (wt%) Size (nm) Phase Content (wt%)
TBT 5.97 ± 0.04 95.5 ± 1 - - 6.1 ± 0.3 4.5 ± 0.9
TBT-HIO3_0.5 6.09 ± 0.03 86 ± 1 - - 5.50 ± 0.19 14 ± 1.5
TBT-HIO3_5 5.43 ± 0.03 89 ± 0.5 - - 5.2 ± 0.2 11 ± 1
TBT-HIO3_20 5.14 ± 0.03 96 ± 1 - - 4.0 ± 0.6 3.5 ± 0.5
TBT-HIO3_50 5.70 ± 0.04 68 ± 3.5 9.08 ± 0.17 32 ± 17 - -
TBT-HIO3_75 5.67 ± 0.05 20.5 ± 3.5 6.57 ± 0.09 7± 1.8 - -
TBT-HIO3_100 6.3 ± 0.2 15 ± 3.5 7.45 ± 0.06 85 ± 1 - -