Figure 17.

Figure 17

(a) Representation of the elongation to fracture of the samples taken vertically and horizontally as a function of the arc mode and the manufacturer’s specification of the elongation to fracture of the pure weld metal (dashed line) and (b) the stress–strain diagram for a horizontally taken tensile specimen in the CMT-ADV manufactured structure with dynamic strain ageing.