Skip to main content
. 2020 Jun 27;10(6):1245. doi: 10.3390/nano10061245

Figure 2.

Figure 2

The dependence of the Pb and Bi concentration in electrodeposited films on the deposition duration at current densities of 10 mA/cm2 (A), 15 mA/cm2 (B), and 20 mA/cm2 (C). The insets show the data of energy-dispersive X-ray microanalysis (EDX) analysis.