Skip to main content
. 2020 Jun 27;10(6):1245. doi: 10.3390/nano10061245

Figure 6.

Figure 6

The dependence of films porosity on electrodeposition duration in PE at 10–20 mA/cm2 current density. The inserts show the porosity contrast images for series 3 samples (Dc = 10 mA/cm2).