Skip to main content
. 2020 Jun 27;10(6):1245. doi: 10.3390/nano10061245

Figure 7.

Figure 7

The dependence of the grain size of electrodeposited films on the duration (A—1 s, B—5 s, С—15 s, D—30 s) in a PE at current densities of 10–20 mA/cm2. The insert shows AFM images of the Bi films surface obtained at a current density of 10 mA/cm2 (scan field size is 5 µm by 5 µm).