Top: modulus (MPa) and strain at break (%) for PCL. Middle: modulus (MPa) and strain at break of PLA-printed parts. (af) Illustrative pictures of the horizontally printed specimens with a number of external PLA layers gradually substituted by PCL. Bottom left: modulus (MPa) of the specimens versus de number of PCL shells. Bottom right: strain at break (%). Layer height: 200 μm.