Skip to main content
. 2020 Jun 11;10(6):1150. doi: 10.3390/nano10061150

Table 3.

Debye–Scherrer diameters (nm) calculated from Full Width Half Maximum (FWHM) of the strongest reflection (101) peaks of undoped and Gd/Mn-doped ZnO-NCs.

ZnO ZnO–Gd0.06 ZnO–Gd0.12 ZnO–Gd0.24 Ol-ZnO Ol-ZnO–Gd0.06 Ol-ZnO–Gd0.12 Ol-ZnO–Gd0.24 Ol-ZnO–Mn0.06 Ol-ZnO–Mn0.12 Ol-ZnO–Mn0.24
Debye–Scherrer diameters (nm) 5.70 3.92 3.98 4.10 5.98 5.63 5.70 5.62 7.41 6.65 5.83