. 2020 Apr 13;11(2):26. doi: 10.3390/jfb11020026

Figure 4.

Figure 4

SEM micrograph of (a) Mg bare alloy, (b) TaN coated, (c) CLT coated after immersion into Kokubo for 14 days and (d) EDS analysis of A, (e) Potentiodynamic polarization curves, (f) corrosion rate, (g) pH value for Mg bare alloy, TaN coated and CLT coated Mg alloy and (h) XRD patterns and (i) Schematic demonstration of the corrosion mechanism of CLT coated Mg alloy after immersion in SBF solution for 14 days.