Figure 9.
Voltage time-courses of POM-mediated cathodes (H2|Pt||POM|O2) at a current density of 5.36 mA/cm2 at either 25 °C or 80 °C under O2 or Ar for 0.01 M solutions of (a) H3PMo12O40, (b) H5PV2Mo10O40, and (c) H6PV3Mo9O40. Adapted from ref. 101. Copyright 2016, American Chemical Society.