Skip to main content
. 2020 May 29;12(6):1231. doi: 10.3390/polym12061231

Figure 5.

Figure 5

Contact angle measurements of PFS/MMA thin-film copolymers (circles) and PFS/MMA thin-film blends (squares) formed from spin-coating a 50mg/mL solution in MEK solvent after annealing at 150 °C for 2 h.