Figure 3.

Figure 3

SEM images and size distributions of ball-milled CP particles (a), PCL/PGS scaffold without CP (b) and PCL/PGS scaffold with 1% (c), 2.5% (d), 5% (e) and 10% (f) CP. Scale bars = 1 µm (a) and 10 µm (bf).