Results of the measured force for glass fiber/polyester resin and memory foam.

Memory Foam Density/Thickness
kg/m3/mm
Glass Fiber/Polyester Resin + Memory Foam
80/15 60/20 80/15 60/10 80/15 100/20 100/10 -
No. 1 2 3 4 5 6 7 8
Force F, N 6874.85 5503.41 7286.87 8581.79 7494.84 4767.66 8338.5 9908.1
7204.46 5473.98 6863.08 8281.60 7578.23 5279.74 8201.16 9638.33
7332.98 5603.47 6869.94 8583.75 6788.52 5061.96 7345.73 8946.72
7524.27 5150.25 6710.04 8495.46 7269.21 5368.03 7910.78 9653.04
7425.19 5032.53 7539.97 8911.40 6633.52 5238.54 8175.65 9962.06
Mean x¯, N 7272.35 5352.73 7053.98 8570.80 7152.86 5143.19 7994.37 9621.65
St. dev. S 251.55 246.88 346.06 226.72 422.46 237.65 394.26 404.58