Skip to main content
. 2020 May 27;12(6):1222. doi: 10.3390/polym12061222

Table 6.

Results of measured force for the carbon and aramid fibers with epoxy resin and memory foam.

Memory Foam Density/Thickness
kg/m3/mm
Carbon/Aramid Fibers/Epoxy Resin + Memory Foam
80/15 60/20 80/15 60/10 80/15 100/20 100/10 -
No. 1 2 3 4 5 6 7 8
Force F, N 8870.20 6553.08 8717.17 9770.76 8110.91 6715.93 9422.51 9378.36
8699.51 6780.67 8711.28 9829.62 8152.11 6521.69 9429.37 9770.76
8846.66 6749.28 6825.80 9922.82 8191.35 6665.90 9323.42 9594.18
8558.24 6574.66 8593.56 9776.65 8252.17 6695.33 9158.62 9633.42
8381.66 7043.58 8358.12 10094.49 8063.82 6603.11 9405.83 9339.12
Mean x¯, N 8671.26 6740.25 8241.18 9878.87 8154.07 6640.39 9347.95 9543.17
St. dev., S 204.80 197.60 167.89 135.08 60.12 78.83 114.0 181.21