Figure 1.
Mechanical properties of the hydrogels. (a) Photographs of a hydrogel before and after stretching (v = 25 mm/min). Edit by WPS Office with the version 11.1.0.9513. https://pc.wps.cn/ (b) Tensile stress curves of the hydrogels prepared with different DMAA to AAc molar ratios. (c) Stress–strain curves of hydrogel D50A50U0.2 stretched at different speeds (v = 50, 100, 200, 400 mm/min). (d) Stress–strain curves of the hydrogel (RDMAA/AAc = 50/50) prepared with different UPy molar ratios (c = 0, 0.2%, 0.4%, 0.8%).