Skip to main content
. 2020 Jul 16;11:3561. doi: 10.1038/s41467-020-17370-7

Fig. 8. AMFC performance and stability using PTFE-added electrodes.

Fig. 8

a i-V and i-power density curves (10 mV s−1 forward scans, solid line H2/O2, dashed line H2/Air (CO2 free) at 1 L min−1) of an AMFC with 8% PTFE in the CL and 20% PTFE in the GDL for both the anode and cathode; (b) voltage vs. time at a constant current density of 600 mA cm−2 under H2/Air (CO2 free) flowed at 1 L min−1. The cell was held at 65 °C with both the anode and cathode RH set at 100%. The anode and cathode RHs were slightly adjusted to remove recoverable performance losses during the stability tests. The anode and cathode loading were 0.70 mgPtRu cm−2 and 0.60 mgPt cm−2, respectively. The membrane used was HDPE5. The data is presented without iR-correction.