SEM top-view images showing 12 Pa TiO2 samples with 3 nm of evaporated Au before (a) and after (b) annealing. Panels (c) and (d) show 12 Pa TiO2 samples with 15 nm of evaporated Au, respectively, before (Au continuous layer) and after annealing (completely formed NPs).