Skip to main content
. 2020 Jul 1;13(13):2954. doi: 10.3390/ma13132954

Figure 2.

Figure 2

(a) N2 gas adsorption-desorption isotherms at 77 K and (b) pore size distribution for Zr(OH)4/GO nanocomposite and pristine Zr(OH)4. All samples were degassed at 393 K under 133 mbar before measurement to eliminate impurities in pores. Pore size distribution was analyzed by using the Barrett–Joyner–Halenda (BJH) method based on Kelvin equation.