Skip to main content
. 2020 Jul 6;13(13):3015. doi: 10.3390/ma13133015

Figure 16.

Figure 16

Figure 16

The voltage change ratio and pressure stress of different rGO–mortars under six-cycle loading (a) 0 wt.% rGO, (b) 0.05 wt.% rGO, (c) 0.5 wt.% rGO, (d) 1.0 wt.% rGO, (e) 2.0 wt.% rGO, (f) 4.0 wt.% rGO.