Table 4.

Properties of cement mortar with different rGO content for 28 d.

Sample rGO Content/% Compressive Strength/MPa Standard
Deviation
Flexural
Strength/MPa
Standard
Deviation
Compressive Strength Increase/% Flexural Strength Increase%
GM0.00 0.00 55.0 4.30 7.8 0.69 - -
GM0.05 0.05 59.7 3.20 8.5 0.45 9 9
GM0.50 0.50 65.5 5.33 8.8 0.70 19 13
GM1.00 1.00 69.2 5.21 9.7 0.47 26 24
GM2.00 2.00 71.0 4.71 10.5 0.80 29 35
GM4.00 4.00 61.1 6.95 9.5 0.82 11 22