Table 2.
Materials used in the pulping (Kraft process).
| Raw material | Process | Chemical used | Conditions |
|---|---|---|---|
| Dried fine chips of SRP (100 g) | Open cooking (2 hours) On electric cooker |
20% NaOH 18% Na2S 1500 ml of HO2 |
Wash in 10 L of freshwater and blending |