Figure 7.
1st cycle voltage profile of cathodes made with only CNT and binder using a) EMIMCl–AlCl3, b) acetalumina and c) uralumina electrolytes. A specific current of 100 mA gc −1 and a voltage range of 0.05–1.85 V was used.