Skip to main content
. 2020 May 15;13(13):3514–3523. doi: 10.1002/cssc.202000447

Figure 10.

Figure 10

Powder XRD diffraction pattern (grazing incidence, incident angle of 5°) of a sulfur cathode with a thickness of 110 μm in the pristine state (black line) and after a full discharge to 0.05 V (red line). The diffraction pattern of crystalline sulfur (blue line) is also shown for comparison, as well as the diffraction pattern of the sample holder (green line).