Skip to main content
. 2020 May 15;13(13):3514–3523. doi: 10.1002/cssc.202000447

Table 3.

Summary of the results of the analysis of the impedance measurements in Figure 6. The errors reported are obtained from the impedance fitting and propagation of experimental errors.

Electrode

R s

[Ω]

CPE‐T

[F sP−1]

CPE‐P

R ct

[Ω]

Wo‐R

[Ω]

Wo‐T

[s]

Wo‐P

Porosity

[%]

MacMullin

number

Tortuosity

thin

≈60 μm

111.2±0.2

(6.5±2.1)×10−5

0.955±0.042

11.6±0.5

47.9±1.8

0.160±0.007

0.484±0.005

81±6

4.0±0.3

3.2±0.4

medium

≈120 μm

100.6±0.1

(8.4±1.9)×10−5

0.982±0.031

10.8±0.3

114.7±1.5

0.707±0.011

0.479±0.001

82±3

4.8±0.2

3.9±0.2

thick

≈190 μm

109.1±0.3

(1.02±0.45)×10−4

0.909±0.060

12.0±0.7

173.8±3.6

0.730±0.018

0.466±0.001

88±2

4.6±0.2

4.1±0.2