Figure 2

Trend of polymer degradation on the sample surface of paint samples aged for 1 up to 6 weeks detected with FT-IR (sum of C-H stretch at 2930 cm-1, C=O stretch at 1730 cm−1, and C–O stretch at 1100 cm−1) and detected using the C2 swan band from LIBS measurements.