Skip to main content
. 2020 Jul 7;12(7):1509. doi: 10.3390/polym12071509

Figure 5.

Figure 5

SEM images of M7, M8 and M9 membranes prepared with PVDF, PVP, PEG, GO and TEP and exposed to humidity for 0, 2.5 and 5 min, respectively. Magnification: top surface 10,000×, cross section 1000×.